F10-F220 Kev Sib Txhuam thiab Kev Sib Tsoo Dub Silicon Carbide Grit
Kawm Ntxiv- Khoom siv:Sic
- Qhov ceev ntawm cov khoom loj:1.45-1.56g/cm3
- Qhov ceev ntawm Ture:3.12 g/cm3
- Loj:F12-F220
- Xim:Dub
- Puab:Cov xuab zeb granular
- Cov ntsiab lus SiC:>98%
- Kev Siv:Polishing. Sib tsoo thiab Sandblasting
- Cov txheej txheem siv lead ua:Lub duab peb ceg
-
Hmoov Silicon Carbide Ntsuab
Kawm Ntxiv- Xim:Ntsuab
- Cov Ntsiab Lus:>98%
- Cov Khoom Siv Tseem Ceeb:α-SiC
- Daim ntawv siv lead ua:Siv lead ua hexagonal
- Mohs hardness:3300kg/mm3
- Qhov ceev tiag tiag:3.2g/hli
- Qhov ceev ntawm cov khoom loj:1.2-1.6g/mm3
- Lub zog tshwj xeeb:3.20-3.25
-
Xim av Fused Aluminium Oxide Grit
Kawm Ntxiv- (Al2O2):≈ 95.5%
- Melting point:2,000° C
- (SiO2) Tsis Muaj Dawb:0.67%
- (Fe2):0.25%
- Daim Ntawv Siv Crystal:Alpha Alumina
- Lub Zog Tshwj Xeeb:3.95 grm/cc
- Qhov Ceev Ntau:132 lbs/ ft3 (nyob ntawm qhov loj)
- Qhov nyuaj::KNOPPS = 2000, MOHS = 9
- Melting Point:2,000° C
-
WFA Dawb Aluminium Oxide Hmoov
Kawm Ntxiv- Xim:Dawb Huv
- Puab:Cubic thiab Angular thiab Ntse
- Lub Zog Tshwj Xeeb:≥ 3.95
- Mohs Hardness:9.2 Mohs
- Melting point:2150 ℃
- Qhov ceev ntawm cov khoom loj:1.50-1.95g/cm3
- Al2O3:99.4% Min
- Na2O:0.30% Max
-
Alumina hmoov rau polishing
Kawm Ntxiv- Xim:Dawb
- Puab:Hmoov
- Khoom siv:Al2O3
- Daim ntawv siv lead ua:Trigonal Crystal System
- Qhov ceev tiag tiag:3.90 g/cm3
- Melting point:2250 °C
- Qhov kub siab tshaj plaws ua haujlwm:1900 °C
- Mohs hardness:9.0-9.5
- Qhov nyuaj me me:2000 - 2200 kg/mm2
-
Kev Sib Tsoo Blasting Polishing Media 240 # -12500 # Dawb Fused Alumina Hmoov
Kawm Ntxiv- Xim:Dawb Huv
- Puab:Cubic thiab Angular thiab Ntse
- Lub Zog Tshwj Xeeb:≥ 3.95
- Mohs Hardness:9.2 Mohs
- Melting point:2150 ℃
- Qhov ceev ntawm cov khoom loj:1.50-1.95g/cm3
- Al2O3:99.4% Min
- Na2O:0.30% Max